HEAT TREATMENT Hardening For maximum hardness (66 Rockwell "C" or 950 D.P.N.), heat to 770°;-790°;C (1420°;-1450°;F). Soak until uniform then quench in clean water or preferably 10% brine solution. The most satisfactory and efficient method is to heat in a salt bath and it is advisable that the temperature should be carefully controlled. The use of a pyrometer is suggested. If a muffle furnace is used the atmosphere should be slightly reducing to minimise scaling and to avoid spots. Supplied in 1 metre lengths. Tempering Minimum 1 hour soak, immediately after hardening.||||Annealing Heat slowly to 760°;-780°;C (1400°;-1469°;F). Soak for 1 hour per inch of section and cool slowly in the furnace.||

Delivery Information

All of our products are stocked in New Zealand, and shipped from our Auckland warehouse, this means no unexpected import fees or taxes.

Why Shop With Smartfox?

With over 20 years of online retail experience, Smartfox is 100% Kiwi owned and operated, backed by 100,000+ customer ratings and 98% positive feedback.

Payment & Security

Payment methods

  • American Express
  • Apple Pay
  • Google Pay
  • Mastercard
  • PayPal
  • Shop Pay
  • Union Pay
  • Visa

Your payment information is processed securely. We do not store credit card details nor have access to your credit card information.

BLACKWOODS

STEEL SILVER 1 MTR LGTH 6.0MM-0.236

$66.90
TECHNICAL SPECIFICATIONS
TERM
DESCRIPTION
Specification 1
HEAT TREATMENT Hardening For maximum hardness (66 Rockwell "C" or 950 D.P.N.), heat to 770°;-790°;C (1420°;-1450°;F). Soak until uniform then quench in clean water or preferably 10% brine solution. The most satisfactory and efficient method is to heat in a salt bath and it is advisable that the temperature should be carefully controlled. The use of a pyrometer is suggested. If a muffle furnace is used the atmosphere should be slightly reducing to minimise scaling and to avoid spots. Supplied in 1 metre lengths. Tempering Minimum 1 hour soak, immediately after hardening.||||Annealing Heat slowly to 760°;-780°;C (1400°;-1469°;F). Soak for 1 hour per inch of section and cool slowly in the furnace.||

Default

  • Default
View product